High-Temp Molten Salt Pump — Bearing Locking
Molten salt pump at 450°C, shaft 65mm, 1500rpm. Special alloy bearings suffered frequent seizure, 3-month average life.
Custom high-purity carbon graphite bearings with antimony impregnation, optimized clearance for 450°C operation.